SABIC® PP G1620B

Want to keep this datasheet? Save it now in your required format

Description

SABIC®PPcompound G1620B is a low flow PP random co-polymer with glass fibers for multi-layer PPR-GF composite pipe applications. This material has been designed to combine a good performance properties with good processing and excellent surface esthetics. SABIC®PPcompound G1620B is a designated pipe grade.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.03 g/cm³

Show Material materials with Density of 1.03 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

3 GPa

Show Material materials with Flexural modulus of 3 GPa

ISO 178

Technological properties

Property
Application areas

Pipe

Fillers

Glass Fiber