Description

SABIC® POM MV 002 is a Polyoxymethylene copolymer grade with medium-viscosity, used for general-purpose injection molded applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.41 g/cm³

Show Material materials with Density of 1.41 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.6 GPa

Show Material materials with Elastic modulus of 2.6 GPa

ISO 527-2 1A | 1mm/min

Elongation at yield

23.0 °C

9 %

Show Material materials with Elongation at yield of 9 %

ISO 527-2 1A

Impact strength, Charpy notched

23.0 °C

5.6 kJ/m²

Show Material materials with Impact strength, Charpy notched of 5.6 kJ/m²

ISO 179

Yield strength

23.0 °C

63 MPa

Show Material materials with Yield strength of 63 MPa

ISO 527-2 1A | 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

100 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 100 °C

ISO 75-1&2 | 1.8 MPa

Melting point

165 °C

Show Material materials with Melting point of 165 °C

ISO 11357-1/-3

Rheological Properties

PropertyValueComment

Melt volume-flow rate

8 cm³/10min

Show Material materials with Melt volume-flow rate of 8 cm³/10min

ISO 1133

Technological properties