SABIC® Vestolen A Rely 5923R 10000 Black

Want to keep this datasheet? Save it now in your required format

Description

SABIC® Vestolen A RELY 5923R 10000 is a grade which has a high density and a bimodal distribution of the molecular mass. Due to its profile of properties this material is typically used for gas and drinking water piping. This material meets (inter)national standards for use in gas, drinking water and waste water piping. MRS class ISO 12162 MPa = 10.0 (PE 100). This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.96 g/cm³

Show Material materials with Density of 0.96 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

62 [-]

Show Material materials with Hardness, Shore D of 62 [-]

ISO 868

Technological properties

Property
Application areas

It is used for gas and drinking water piping. This material meets (inter)national standards for use in gas, drinking water and waste water piping.