SABIC® Vestolen A RELY 5924R 10000 Black

Want to keep this datasheet? Save it now in your required format

Description

SABIC® Vestolen A RELY 5924R 10000 is a grade which has a high density and a bimodal distribution of the molecular mass. Due to the low sag characteristics of this material it may be used for the production of thick walled (large diameter and low SDR) pipes for infrastructure and industrial applications and shows favorable processing behaviour. This material meets (inter)national standards for use in gas, drinking water and waste water piping. MRS class ISO 12162 MPa = 10.0 (PE 100). This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.96 g/cm³

Show Material materials with Density of 0.96 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Hardness, Shore D

23.0 °C

63 [-]

Show Material materials with Hardness, Shore D of 63 [-]

ISO 868

Technological properties

Property
Application areas

It is used for no dig applications. Also used for the production of thick walled (large diameter and low SDR) pipes for infrastructure and industrial application. This material meets (inter)national standards for use in gas, drinking water and waste water piping.

Color

Black