Crastin® SK692FR NC010

Alternative and trade names
PBT-GF15FR(17)
Want to keep this datasheet? Save it now in your required format

Description

Common features of Crastin® thermoplastic polyester resin include mechanical and physical properties such as stiffness and toughness, heat resistance, friction and wear resistance, excellent surface finishes and good colourability. Crastin® thermoplastic polyester resin has excellent electrical insulation characteristics and high arc-resistant grades are available. Many flame retardant grades have UL recognition (class V-0). Crastin® thermoplastic polyester resin typically has high chemical and heat ageing resistance.The good melt stability of Crastin® thermoplastic polyester resin normally enables the recycling of properly handled production waste. If recycling is not possible, DuPont recommends, as the preferred option, incineration with energy recovery (24 kJ/g of base polymer) in appropriately equipped installations. For disposal, local regulations have to be observed. Crastin® thermoplastic polyester resin typically is used in demanding applications in the electronics, electrical, automotive, mechanical engineering, chemical, domestic appliances and sporting goods industry.Crastin® SK692FR is a 15% glass reinforced, flame retardant polybutylene terephtalate for injection moulding.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.55 g/cm³

Show Material materials with Density of 1.55 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

7 GPa

Show Material materials with Elastic modulus of 7 GPa

ISO 527-1/-2

Elongation

23.0 °C

2.7 %

Show Material materials with Elongation of 2.7 %

ISO 527-1/-2

Impact strength, Charpy notched

23.0 °C

6.8 kJ/m²

Show Material materials with Impact strength, Charpy notched of 6.8 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

23.0 °C

38 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 38 kJ/m²

ISO 179/1eU

Poisson's ratio

23.0 °C

0.35 [-]

Show Material materials with Poisson's ratio of 0.35 [-]

Tensile strength

23.0 °C

115 MPa

Show Material materials with Tensile strength of 115 MPa

ISO 527-1/-2

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

199 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 199 °C

ISO 75-1/-2

Melting point

223 °C

Show Material materials with Melting point of 223 °C

ISO 11357-1/-3 | 18°F/min

Relative temperature index, electrical

130 °C

Show Material materials with Relative temperature index, electrical of 130 °C

UL 746B | 120mil

Relative temperature index, mechanical impact

130 °C

Show Material materials with Relative temperature index, mechanical impact of 130 °C

UL 746B | 120mil

Relative temperature index, mechanical strength

130 °C

Show Material materials with Relative temperature index, mechanical strength of 130 °C

UL 746B | 120mil

Flammability

Burning Behav. at 60mil nom. thickn.: V-0 class, Thickness tested: 1.5 mm, UL recognition: yes -, Burning Behav. at thickness h: V-0 class, Thickness tested: 0.75 mm, UL recognition: yes -, Glow Wire Flammability Index, 120mil: 960 °C, Glow Wire Ignition Temperature, 120mil: 725 °C, FMVSS Class: DNI -

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

175 V

Show Material materials with Comparative tracking index of 175 V

IEC 60112

Dielectric strength

23.0 °C

35 kV/mm

Show Material materials with Dielectric strength of 35 kV/mm

IEC 60243-1

Surface resistivity

23.0 °C

1.00E+15 Ω/sq

Show Material materials with Surface resistivity of 1.00E+15 Ω/sq

min. | IEC 62631-3-2

Volume resistivity

23.0 °C

1.00E+15 Ω·cm

Show Material materials with Volume resistivity of 1.00E+15 Ω·cm

min. | IEC 62631-3-1

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.7 %

Show Material materials with Shrinkage of 0.7 %

ISO 294-4, 2577

Shrinkage, transverse

23.0 °C

1 %

Show Material materials with Shrinkage, transverse of 1 %

ISO 294-4, 2577

Technological properties

Property
Fillers

15% Glass Fiber

Processing methods

Drying Recommended: yes, Drying Temperature: 120°C, Drying Time, Dehumidified Dryer: 2-4h, Processing Moisture Content: ≤0.04%, Melt Temperature Optimum: 250°C, Min. melt temperature: 240°C, Max. melt temperature: 260°C, Mold Temperature Optimum: 80°C, Min. mold temperature: 30°C, Max. mold temperature: 130°C, Hold pressure range: ≥60MPa, Hold pressure time: 3s/mm, Back pressure: As low as possible, Ejection temperature: 170°C