TPSiV® 5300 A6002

Want to keep this datasheet? Save it now in your required format

Description

TPSiV® thermoplastic elastomers combine the strength, toughness and abrasion resistance of any thermoplastic elastomer with the desirable properties of silicone: softness, silky feel, resistance to UV light and chemicals, and outstanding colorability. These unique materials incorporate vulcanized silicone modules in a thermoplastic matrix, but unlike traditional thermoplastic vulcanizates (TPVs), they can be recycled and reused in your manufacturing processes.TPSiV® 5300 A6002 thermoplastic elastomer is a low odor, plasticizer-free thermoplastic elastomer with excellent bonding to polypropylene and polyethylene. It is a product targeted for soft touch overmolding on wearable electronics, accessory cases for consumer electronics and flexible pipe connectors in potable water systems.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

845 %

Show Material materials with Elongation of 845 %

ISO 527-1/-2

Hardness, Shore A

23.0 °C

60 [-]

Show Material materials with Hardness, Shore A of 60 [-]

ISO 7619-1 | 3 seconds

Tear strength, transverse

23.0 °C

44 kN/m

Show Material materials with Tear strength, transverse of 44 kN/m

ISO 34-1

Tensile strength

23.0 °C

7.4 MPa

Show Material materials with Tensile strength of 7.4 MPa

ISO 527-1/-2

Technological properties

Property
Processing methods

Drying Recommended: no, Mold Temperature Optimum: 30°C, Min. mold temperature: 28°C, Max. mold temperature: 32°C