General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.74 g/cm³ Show Material materials with Density of 8.74 g/cm³ |
Dimension
Property | Value | Comment | |
---|---|---|---|
Length | 3050 - 3660 mm Show Material materials with Length of 3050 - 3660 mm | Mill random length | |
Width | 3.2 - 31.8 mm Show Material materials with Width of 3.2 - 31.8 mm | ||
Dimensions | Available widths: 3.2mm, 3.6mm, 6.4mm, 12.7mm, 15.9mm, 19.1mm, 25.4mm, 31.8mm |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 217 GPa Show Material materials with Elastic modulus of 217 GPa | |
Elongation | 23.0 °C | 40 % Show Material materials with Elongation of 40 % | in 2 in. |
Hardness, Rockwell B | 23.0 °C | 85 [-] Show Material materials with Hardness, Rockwell B of 85 [-] | |
Tensile strength | 23.0 °C | 676 MPa Show Material materials with Tensile strength of 676 MPa | |
Yield strength | 23.0 °C | 262 MPa Show Material materials with Yield strength of 262 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 450.0 °C | 1.36E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.36E-5 1/K | from 20°C to the mentioned temperature |
Melting point | 1454 °C Show Material materials with Melting point of 1454 °C | ||
Specific heat capacity | 23.0 °C | 460 J/(kg·K) Show Material materials with Specific heat capacity of 460 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 35 W/(m·K) Show Material materials with Thermal conductivity of 35 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 5.9E-7 Ω·m Show Material materials with Electrical resistivity of 5.9E-7 Ω·m |
Magnetic
Property | Temperature | Value |
---|---|---|
Coercive force | 23.0 °C | 1.19 A/m Show Material materials with Coercive force of 1.19 A/m |
Curie temperature | 460 °C Show Material materials with Curie temperature of 460 °C | |
Relative magnetic permeability | 23.0 °C | 230000 [-] Show Material materials with Relative magnetic permeability of 230000 [-] |
Saturation induction | 23.0 °C | 0.8 T Show Material materials with Saturation induction of 0.8 T |
Chemical properties
Property | Value |
---|---|
Carbon | 0.03 % Show Material materials with Carbon of 0.03 % |
Iron | Balance |
Manganese | 0.95 % Show Material materials with Manganese of 0.95 % |
Molybdenum | 5 % Show Material materials with Molybdenum of 5 % |
Nickel | 80 % Show Material materials with Nickel of 80 % |
Phosphorus | 0.02 % Show Material materials with Phosphorus of 0.02 % |
Silicon | 0.42 % Show Material materials with Silicon of 0.42 % |
Sulfur | 8E-3 % Show Material materials with Sulfur of 8E-3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Common applications of EFI ALLOY 79 are: Toroidal tape-wound cores - instrument transformers, inductive components, earth-leakage circuit breakers; Magnetic shielding - shielding cans, shielding films, spatial shielding arrangements; Ground fault circuit interrupters; Electromagnetic relay parts; Laminations - transformer laminations, transformer cores for modems, stampled rings for electronic earth-leakage breakers, operating at a low magnetic field strengths |