General
Property | Value | Temperature |
---|---|---|
Density | 10.28 g/cm³ Show Material materials with Density of 10.28 g/cm³ at 23.0 °C | 23.0 °C |
Dimension
Property | Value |
---|---|
Dimensions | Available thicknesses: 0.13mm, 0.18mm, 0.25mm, 0.38mm, 0.51mm, 0.64mm, 0.76mm, 1.02mm, 5.08mm, 0.64mm, 0.76mm, 1.02mm, 1.27mm, 1.52mm, 1.59mm, 2.03mm, 2.29mm, 3.18mm |
Thickness | 0.13 - 3.18 mm Show Material materials with Thickness of 0.13 - 3.18 mm |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Elastic modulus | 320 GPa Show Material materials with Elastic modulus of 320 GPa at 23.0 °C | 23.0 °C | |
Elongation | 12 % Show Material materials with Elongation of 12 % at 23.0 °C | 23.0 °C | in 1 in. |
Hardness, Vickers | 220 [-] Show Material materials with Hardness, Vickers of 220 [-] at 23.0 °C | 23.0 °C | |
Tensile strength | 1035 MPa Show Material materials with Tensile strength of 1035 MPa at 20.0 °C | 20.0 °C | |
515 MPa Show Material materials with Tensile strength of 515 MPa at 500.0 °C | 500.0 °C | ||
175 MPa Show Material materials with Tensile strength of 175 MPa at 1000.0 °C | 1000.0 °C | ||
Thermal
Property | Value | Temperature |
---|---|---|
Coefficient of thermal expansion | 4.8E-6 1/K Show Material materials with Coefficient of thermal expansion of 4.8E-6 1/K at 23.0 °C | 23.0 °C |
Crystallization temperature | 1100 °C Show Material materials with Crystallization temperature of 1100 °C | |
Melting point | 2623 °C Show Material materials with Melting point of 2623 °C | |
Specific heat capacity | 259 J/(kg·K) Show Material materials with Specific heat capacity of 259 J/(kg·K) at 23.0 °C | 23.0 °C |
Thermal conductivity | 142 W/(m·K) Show Material materials with Thermal conductivity of 142 W/(m·K) at 23.0 °C | 23.0 °C |
Electrical
Property | Value | Temperature |
---|---|---|
Electrical resistivity | 5.34E-8 Ω·m Show Material materials with Electrical resistivity of 5.34E-8 Ω·m at 200.0 °C | 200.0 °C |
Chemical properties
Property | ||
---|---|---|
Molybdenum | 99.97 % | min |
Technological properties
Property | ||
---|---|---|
Application areas | In the missile industry Molybdenum is used for nose cones, high temperature structural parts, nozzles, leading edges of control surfaces, support vanes, re-entry cones, and heat radiation shields. In electronics Molybdenum is used for cathodes, magnetron end hats, x-ray tube components, filaments, and glass-to-metal seals. In high-temperature applications Molybdenum is used for: furnace windings, structural furnace members, and containers for components exposed to high temperatures. |