General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8.05 g/cm³ Show Material materials with Density of 8.05 g/cm³ |
Dimension
Property | Value |
---|---|
Length | 914 - 1828 mm Show Material materials with Length of 914 - 1828 mm |
Thickness | 3.8 - 88.9 mm Show Material materials with Thickness of 3.8 - 88.9 mm |
Width | 381 - 508 mm Show Material materials with Width of 381 - 508 mm |
Dimensions | Available dimensions (mm x mm x mm): 3.8 x 381.0 x 914.4, 4.8 x 381.0 x 1828.8, 6.4 x 381.0 x 1828.8, 9.5 x 508.0 x 1828.8, 12.7 x 508.0 x 1828.8, 15.9 x 508.0 x 1828.8, 19.1 x 381.0 x 1828.8, 25.4 x 381.0 x 1828.8, 31.8 x 457.2 x 1828.8, 38.1 x 508.0 x 1828.8, 44.5 x 508.0 x 1828.8, 50.8 x 508.0 x 1828.8, 57.2 x 457.2 x 1828.8, 63.5 x 457.2 x 1828.8, 76.2 x 508.0 x 1828.8, 88.9 x 457.2 x 1828.8 |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 141 GPa Show Material materials with Elastic modulus of 141 GPa | |
Elongation | 23.0 °C | 34 % Show Material materials with Elongation of 34 % | in 2 in. |
Hardness, Rockwell B | 23.0 °C | 80 [-] Show Material materials with Hardness, Rockwell B of 80 [-] | |
Poisson's ratio | 23.0 °C | 0.29 [-] Show Material materials with Poisson's ratio of 0.29 [-] | |
Tensile strength | 23.0 °C | 518 MPa Show Material materials with Tensile strength of 518 MPa | |
Yield strength | 23.0 °C | 276 MPa Show Material materials with Yield strength of 276 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.9E-6 1/K Show Material materials with Coefficient of thermal expansion of 1.9E-6 1/K | from 20°C to the mentioned temperature |
150.0 °C | 2.4E-6 1/K Show Material materials with Coefficient of thermal expansion of 2.4E-6 1/K | from 20°C to the mentioned temperature | |
200.0 °C | 3E-6 1/K Show Material materials with Coefficient of thermal expansion of 3E-6 1/K | from 20°C to the mentioned temperature | |
250.0 °C | 4.4E-6 1/K Show Material materials with Coefficient of thermal expansion of 4.4E-6 1/K | from 20°C to the mentioned temperature | |
300.0 °C | 6.1E-6 1/K Show Material materials with Coefficient of thermal expansion of 6.1E-6 1/K | from 20°C to the mentioned temperature | |
350.0 °C | 7.5E-6 1/K Show Material materials with Coefficient of thermal expansion of 7.5E-6 1/K | from 20°C to the mentioned temperature | |
400.0 °C | 8.7E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.7E-6 1/K | from 20°C to the mentioned temperature | |
450.0 °C | 8.9E-6 1/K Show Material materials with Coefficient of thermal expansion of 8.9E-6 1/K | from 20°C to the mentioned temperature | |
500.0 °C | 1.05E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.05E-5 1/K | from 20°C to the mentioned temperature | |
600.0 °C | 1.18E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.18E-5 1/K | from 20°C to the mentioned temperature | |
Melting point | 1427 °C Show Material materials with Melting point of 1427 °C | ||
Specific heat capacity | 23.0 °C | 502 J/(kg·K) Show Material materials with Specific heat capacity of 502 J/(kg·K) | |
Thermal conductivity | 23.0 °C | 10 W/(m·K) Show Material materials with Thermal conductivity of 10 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical resistivity | 23.0 °C | 8.2E-7 Ω·m Show Material materials with Electrical resistivity of 8.2E-7 Ω·m |
Magnetic
Property | Value |
---|---|
Curie temperature | 279 °C Show Material materials with Curie temperature of 279 °C |
Chemical properties
Property | Value |
---|---|
Carbon | 0.05 % Show Material materials with Carbon of 0.05 % |
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % |
Cobalt | 0.5 % Show Material materials with Cobalt of 0.5 % |
Iron | Balance |
Nickel | 36 % Show Material materials with Nickel of 36 % |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % |
Sulfur | 0.015 % Show Material materials with Sulfur of 0.015 % |
Technological properties
Property | ||
---|---|---|
Application areas | Positioning devices • Bimetal thermostats • Advanced composite molds for aerospace industry • Dimensionally stable instruments and optical devices • Containers for LNG tankers • Transfer lines for LNG • Echo boxes and filters for mobile telephones • Magnetic shielding • Small electrical transformers • Metrology devices • Scientific instruments • Electrical circuit breakers • Temperature regulators • Clock balance wheels • Pendulum clocks • Precision condenser blades • Radar and microwave cavity resonators • Special electronic housings • Seals, spacers, and specialized frames • High voltage transmission lines • CRT applications: shadow masks, deflection clips, and electron gun components. |