Description

State-of-the-art chemical vapour deposition (CVD) methods produce exceptionally high quality graphene film for use as transparent conductors and in other innovative applications.


This material data has been provided by Matmatch.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Domain size

10 - 20 μm

Show Material materials with Domain size of 10 - 20 μm

Substrate

PET, 188µm

Dimension

PropertyValueComment

Length

600 mm

Show Material materials with Length of 600 mm

max

Width

500 mm

Show Material materials with Width of 500 mm

max

Electrical

PropertyTemperatureValue

Carrier mobility

23.0 °C

3500 cm²/Vs

Show Material materials with Carrier mobility of 3500 cm²/Vs

Surface resistivity

23.0 °C

250 - 400 Ω/sq

Show Material materials with Surface resistivity of 250 - 400 Ω/sq

Optical

PropertyValue

Luminous transmittance

97 [-]

Show Material materials with Luminous transmittance of 97 [-]

Technological properties

Property
Application areas

Light flexible displays, plastic electronics, printed circuit boards, liquid crystal displays, thin film photovoltaics, e-paper, sensors and OLEDs

Processing history

Growth method: CVD