The material: 'TYÜP BMF 0117' you were looking for has been superseded by the one below.

Biopolymer TYÜP BMF 0117

Want to keep this datasheet? Save it now in your required format

Description

Blow Extrusion grade bio resin & industrial compostable.

This material data has been provided by Indochine Bio Plastiques (ICBP) Sdn. Bhd..

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Bio-based content

100 %

Show Material materials with Bio-based content of 100 %

Density

1.26 - 1.3 g/cm³

Show Material materials with Density of 1.26 - 1.3 g/cm³

Mechanical

PropertyValueComment

Elongation

300.0 %

Show Material materials with Elongation of 300.0 %

min.

Tensile strength

15 MPa

Show Material materials with Tensile strength of 15 MPa

min.

Thermal

PropertyValue

Melting point

110.0 - 120.0 °C

Show Material materials with Melting point of 110.0 - 120.0 °C

Rheological Properties

PropertyValueComment

Melt mass-flow rate

3 g/10min

Show Material materials with Melt mass-flow rate of 3 g/10min

190°C/2.16kg

5 g/10min

Show Material materials with Melt mass-flow rate of 5 g/10min

190°C/2.16kg

Technological properties

Property
Application areas

Shopping bag, garbage bag, mulch film, waste bag, food packaging bag

Certifications

Food Contact: Halal

Processing methods

1. Pre-clean the machine with LDPE at original processing temperature. 2. Purge the machine using BMF 0117 at temperature 145-160°C. 3. Barrel temperature should be lowered if the die temperature is too high or the viscosity of the extruded material is too thin. 4. Adjust the cooling air volume to make the bubble smooth and steady.