Description

It is a CuCrZr alloy that can be hardened by cold forming and by precipitation of CuCrZr - phases during a heat treatment. It has good bendability, excellent hot and cold forming properties, a high strength and a good corrosion resistance. Due to the CrZr-precipitations the relaxation properties, even at temperatures up to 250°C are excellent. The electrical and thermal conductivity is excellent. Welding, soldering and brazing properties are good too. The alloy is registered in the US by EPA to have good antimicrobial properties.

Equivalent Materials

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Mechanical

PropertyTemperatureValueComment

Bendability 180°, bw

23.0 °C

2 [-]

Show Material materials with Bendability 180°, bw of 2 [-]

r = x t, t <0.5mm

Bendability 180°, gw

23.0 °C

2 [-]

Show Material materials with Bendability 180°, gw of 2 [-]

r = x t, t <0.5mm

Bendability 90°, bw

23.0 °C

1.5 [-]

Show Material materials with Bendability 90°, bw of 1.5 [-]

r = x t, t <0.5mm

Bendability 90°, gw

23.0 °C

1.5 [-]

Show Material materials with Bendability 90°, gw of 1.5 [-]

r = x t, t <0.5mm

Elastic modulus

23.0 °C

137 GPa

Show Material materials with Elastic modulus of 137 GPa

cold formed

Elongation A50

23.0 °C

8 %

Show Material materials with Elongation A50 of 8 %

Hardness, Vickers

23.0 °C

150 - 190 [-]

Show Material materials with Hardness, Vickers of 150 - 190 [-]

Tensile strength

23.0 °C

480 - 560 MPa

Show Material materials with Tensile strength of 480 - 560 MPa

Yield strength Rp0.2

23.0 °C

450 MPa

Show Material materials with Yield strength Rp0.2 of 450 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

300.0 °C

1.8E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.8E-5 1/K

for 20°C to the mentioned temperature

Specific heat capacity

23.0 °C

381 J/(kg·K)

Show Material materials with Specific heat capacity of 381 J/(kg·K)

Thermal conductivity

23.0 °C

330 W/(m·K)

Show Material materials with Thermal conductivity of 330 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

5.00E+7 - 5.30E+7 S/m

Show Material materials with Electrical conductivity of 5.00E+7 - 5.30E+7 S/m

Specific Electrical conductivity

86 % IACS

Show Material materials with Specific Electrical conductivity of 86 % IACS

Chemical properties

PropertyValueComment

Chromium

0.2 - 1.2 %

Show Material materials with Chromium of 0.2 - 1.2 %

Copper

Balance

Iron

0.1 %

Show Material materials with Iron of 0.1 %

max.

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

max.

Zirconium

0.05 - 0.25 %

Show Material materials with Zirconium of 0.05 - 0.25 %

Technological properties

Property
Application areas

Automotive: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Hybrid Cars. Electrical: Switches and Relays, Contacts, Connectors, Terminals, Press fits, Components for the electrical industry, Stamped parts, Semiconductor Components, Junction Boxes, Photovoltaic Systems.

Brazing

Excellent

Cold Forming

Good

Corrosion properties

STOL® 95 is resistant to pure water vapour and non oxidizingacids and alkalis as well as neutral saline solutions. The material is insensitive to stress corrosion cracking.

Heat Treatment

Temper: R480

Machining

Rating 20, less suitable

Other

This alloy is in accordance with RoHS 2002/96/CE for electric & electronic equipments and 2002/53/CE for automotive industry. It is suitable for high voltage applications as hybrid cars or photovoltaics.

Plating

Electroplating is excellent

Welding

Gas Shielded Arc Welding: Excellent, Laser Welding: Fair