Density
ρ8.21 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.5851E-5 1/K at 23 °C
Coefficient of thermal expansion, transverse
αtrans0.02 1/K at 23 °C
Specific heat capacity
cp455.07 J/(kg·K) at 23 °C
Thermal conductivity
λ101.45 W/(m·K) at 23 °C
Thermal conductivity, transverse
λtrans22.39 W/(m·K) at 23 °C
Electrical conductivity
σel1.35E+7 S/m at 23 °C
Electrical conductivity, transverse
σel, trans1.58E+7 S/m at 23 °C
Electrical resistivity
ρel7.4E-8 Ω·m at 23 °C
Coating
Different coating layers are available upon request.
This material data has been provided by Matmatch.