General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 8 g/cm³ Show Material materials with Density of 8 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Elastic modulus | 23.0 °C | 112.05 GPa Show Material materials with Elastic modulus of 112.05 GPa |
Tensile strength | 23.0 °C | 207.5 MPa Show Material materials with Tensile strength of 207.5 MPa |
Yield strength | 23.0 °C | 99.5 MPa Show Material materials with Yield strength of 99.5 MPa |
Thermal
Property | Temperature | Value |
---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.74E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.74E-5 1/K |
Coefficient of thermal expansion, transverse | 23.0 °C | 0.01 1/K Show Material materials with Coefficient of thermal expansion, transverse of 0.01 1/K |
Specific heat capacity | 23.0 °C | 411.98 J/(kg·K) Show Material materials with Specific heat capacity of 411.98 J/(kg·K) |
Thermal conductivity | 23.0 °C | 368.05 W/(m·K) Show Material materials with Thermal conductivity of 368.05 W/(m·K) |
Thermal conductivity, through-plane | 23.0 °C | 352.6 W/(m·K) Show Material materials with Thermal conductivity, through-plane of 352.6 W/(m·K) |
Electrical
Property | Temperature | Value |
---|---|---|
Electrical conductivity | 23.0 °C | 5.38E+7 S/m Show Material materials with Electrical conductivity of 5.38E+7 S/m |
Electrical conductivity, transverse | 23.0 °C | 1.78E+7 S/m Show Material materials with Electrical conductivity, transverse of 1.78E+7 S/m |
Electrical resistivity | 23.0 °C | 1.9E-8 Ω·m Show Material materials with Electrical resistivity of 1.9E-8 Ω·m |
Technological properties
Property | ||
---|---|---|
Coating | Different coating layers are available upon request. |