Clad material. Check out the clad configurator https://app.wickeder.de for more variants.
See where Al 99.0 / DD11 (10-90) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ7.34 g/cm³ at 23 °C
Coefficient of thermal expansion
α1.096E-5 1/K at 23 °C
Coefficient of thermal expansion, transverse
αtrans1.5E-3 1/K at 23 °C
Specific heat capacity
cp480.96 J/(kg·K) at 23 °C
Thermal conductivity
λ71.5 W/(m·K) at 23 °C
Thermal conductivity, transverse
λtrans59.46 W/(m·K) at 23 °C
Electrical conductivity
σel1.07E+7 S/m at 23 °C
Electrical conductivity, transverse
σel, trans1.18E+7 S/m at 23 °C
Electrical resistivity
ρel9.3E-8 Ω·m at 23 °C
Coating
Different coating layers are available upon request.
This material data has been provided by Matmatch.