The material: 'Ni 99.6 / 1.4310 / Cu-ETP (2-38-60)' you were looking for has been superseded by the one below.

EN 2.4060,EN 1.4310,EN CW004A

Alternative and trade names
SIGMAclad
Want to keep this datasheet? Save it now in your required format

Description

Clad material. Check out the clad configurator https://app.wickeder.de for more variants.

Ashby charts

See where EN 2.4060,EN 1.4310,EN CW004A falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

8.54 - 8.58 g/cm³ at 23 °C

Mechanical

Elastic modulus

E

152.16 - 152.48 GPa at 23 °C

Show Clad / Bimetal materials with Elastic modulus of 152.16 - 152.48 GPa at 23 °C

Tensile strength

Rm

428.5 - 441.5 MPa at 23 °C

Show Clad / Bimetal materials with Tensile strength of 428.5 - 441.5 MPa at 23 °C

Yield strength

YS

168.5 - 173.5 MPa at 23 °C

Show Clad / Bimetal materials with Yield strength of 168.5 - 173.5 MPa at 23 °C

Thermal

Coefficient of thermal expansion

α

1.6132E-5 - 1.6297E-5 1/K at 23 °C

Coefficient of thermal expansion, transverse

αtrans

0.01 - 0.02 1/K at 23 °C

Specific heat capacity

cp

426.93 - 427.83 J/(kg·K) at 23 °C

Thermal conductivity

λ

243.67 - 245.81 W/(m·K) at 23 °C

Thermal conductivity, transverse

λtrans

37.98 - 41.11 W/(m·K) at 23 °C

Electrical

Electrical conductivity

σel

3.50E+7 - 3.54E+7 S/m at 23 °C

Electrical conductivity, transverse

σel, trans

1.63E+7 - 1.64E+7 S/m at 23 °C

Electrical resistivity

ρel

2.8E-8 - 2.9E-8 Ω·m at 23 °C

Technological properties

Coating

Different coating layers are available upon request.

This material data has been provided by Matmatch.