General
Property | Value |
---|---|
Density | 1.03 - 1.05 g/cm³ Show Material materials with Density of 1.03 - 1.05 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 1.5 - 2.9 GPa Show Material materials with Elastic modulus of 1.5 - 2.9 GPa | |
Elongation | 25.0 - 60.0 % Show Material materials with Elongation of 25.0 - 60.0 % | |
Impact strength, Charpy notched | 5.0 - 10.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 5.0 - 10.0 kJ/m² | |
Impact strength, Charpy unnotched | 50 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | |
Tensile strength | 15.0 - 45.0 MPa Show Material materials with Tensile strength of 15.0 - 45.0 MPa | at 2-3% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 7.5e-05 - 0.0001 1/K Show Material materials with Coefficient of thermal expansion of 7.5e-05 - 0.0001 1/K |
Specific heat capacity | 1300 J/(kg·K) Show Material materials with Specific heat capacity of 1300 J/(kg·K) |
Thermal conductivity | 0.16 - 0.18 W/(m·K) Show Material materials with Thermal conductivity of 0.16 - 0.18 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.4 [-] Show Material materials with Dielectric constant of 2.4 [-] |
2.6 [-] Show Material materials with Dielectric constant of 2.6 [-] | |
Electrical resistivity | 100000000000000 Ω·m Show Material materials with Electrical resistivity of 100000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Housewares, electrical housings, drink cups, deli-trays, internal fittings refrigerators | |
Processing methods | Injection molding, blow molding, extrusion, thermoforming |