Styrene butadiene Copolymer (SBC)

Alternative and trade names
Styrolux®, Elastamax™, Sofprene®
Want to keep this datasheet? Save it now in your required format

Description

SB has the combination of high transparency, brilliance and impact resistance. The good miscibility of it and polystyrene allows adjustment to the desired toughness, while at the same time reducing material costs. The key features are:


  • Transparency
  • Low temperature toughness
  • Flowability
  • Impact strength
  • High elastic recovery both at low and room temperature
  • Excellent resistance to several chemical agents, i.e. bases, acids, alcohols, detergents, water solutions
  • High thermal and electric insulation values
  • Good abrasion resistance
  • This material data has been provided by M-Base.

    "Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.03 - 1.05 g/cm³

    Show Material materials with Density of 1.03 - 1.05 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    1.5 - 2.9 GPa

    Show Material materials with Elastic modulus of 1.5 - 2.9 GPa

    Elongation

    25.0 - 60.0 %

    Show Material materials with Elongation of 25.0 - 60.0 %

    Impact strength, Charpy notched

    5.0 - 10.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 5.0 - 10.0 kJ/m²

    Impact strength, Charpy unnotched

    50 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

    Tensile strength

    15.0 - 45.0 MPa

    Show Material materials with Tensile strength of 15.0 - 45.0 MPa

    at 2-3% strain

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    7.5e-05 - 0.0001 1/K

    Show Material materials with Coefficient of thermal expansion of 7.5e-05 - 0.0001 1/K

    Specific heat capacity

    1300 J/(kg·K)

    Show Material materials with Specific heat capacity of 1300 J/(kg·K)

    Thermal conductivity

    0.16 - 0.18 W/(m·K)

    Show Material materials with Thermal conductivity of 0.16 - 0.18 W/(m·K)

    Flammability

    UL 94 HB

    Electrical

    PropertyValue

    Dielectric constant

    2.4 [-]

    Show Material materials with Dielectric constant of 2.4 [-]

    2.6 [-]

    Show Material materials with Dielectric constant of 2.6 [-]

    Electrical resistivity

    100000000000000 Ω·m

    Show Material materials with Electrical resistivity of 100000000000000 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Application areas

    Housewares, electrical housings, drink cups, deli-trays, internal fittings refrigerators

    Processing methods

    Injection molding, blow molding, extrusion, thermoforming