Plasticized Polyvinyl chloride, plasticized (PPVC)

Alternative and trade names
Inovyn™, Vestolit, Vinnolit
Want to keep this datasheet? Save it now in your required format

This material data has been provided by M-Base.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.16 - 1.35 g/cm³

Show Material materials with Density of 1.16 - 1.35 g/cm³

Mechanical

PropertyValueComment

Elongation

170.0 - 500.0 %

Show Material materials with Elongation of 170.0 - 500.0 %

Tensile strength

5.0 - 28.0 MPa

Show Material materials with Tensile strength of 5.0 - 28.0 MPa

at 170-500% strain

Impact strength, Charpy notched

no break

Impact strength, Charpy unnotched

no break

Thermal

PropertyValue

Coefficient of thermal expansion

0.00015 - 0.00021 1/K

Show Material materials with Coefficient of thermal expansion of 0.00015 - 0.00021 1/K

Specific heat capacity

900.0 - 1800.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 - 1800.0 J/(kg·K)

Thermal conductivity

0.15 W/(m·K)

Show Material materials with Thermal conductivity of 0.15 W/(m·K)

Electrical

PropertyValue

Dielectric constant

3 [-]

Show Material materials with Dielectric constant of 3 [-]

4.8 [-]

Show Material materials with Dielectric constant of 4.8 [-]

Electrical resistivity

1000000000.0 - 10000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000.0 - 10000000000000.0 Ω·m

Technological properties

Property
Application areas

Pipes, tubes, hand rail profiles, cable- and wire sheathing, floor coverings

Processing methods

Injection molding, blow molding, extrusion, coating, calandering