General
Property | Value |
---|---|
Density | 1.76 - 1.78 g/cm³ Show Material materials with Density of 1.76 - 1.78 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 2 - 3 GPa Show Material materials with Elastic modulus of 2 - 3 GPa | ||
Elongation | 100 - 400 % Show Material materials with Elongation of 100 - 400 % | ||
Tensile strength | 45 - 60 MPa Show Material materials with Tensile strength of 45 - 60 MPa | at 7-10% strain | |
Impact strength, Charpy notched | no break | ||
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.0001 - 0.00016 1/K Show Material materials with Coefficient of thermal expansion of 0.0001 - 0.00016 1/K |
Melting point | 160 - 175 °C Show Material materials with Melting point of 160 - 175 °C |
Specific heat capacity | 1170 - 1500 J/(kg·K) Show Material materials with Specific heat capacity of 1170 - 1500 J/(kg·K) |
Thermal conductivity | 0.14 - 0.19 W/(m·K) Show Material materials with Thermal conductivity of 0.14 - 0.19 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Membranes, pump parts, valve parts, pipes, shrink tubes | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, extrusion, coating |