General
Property | Value |
---|---|
Density | 1.24 - 1.25 g/cm³ Show Material materials with Density of 1.24 - 1.25 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 2.5 - 2.8 GPa Show Material materials with Elastic modulus of 2.5 - 2.8 GPa | ||
Elongation | 25.0 - 30.0 % Show Material materials with Elongation of 25.0 - 30.0 % | ||
Impact strength, Charpy notched | 3.5 - 7.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 3.5 - 7.0 kJ/m² | ||
Tensile strength | 70.0 - 90.0 MPa Show Material materials with Tensile strength of 70.0 - 90.0 MPa | at 6-22% strain | |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 5.5e-05 - 6e-05 1/K Show Material materials with Coefficient of thermal expansion of 5.5e-05 - 6e-05 1/K |
Specific heat capacity | 1300 J/(kg·K) Show Material materials with Specific heat capacity of 1300 J/(kg·K) |
Thermal conductivity | 0.15 - 0.28 W/(m·K) Show Material materials with Thermal conductivity of 0.15 - 0.28 W/(m·K) |
Flammability | UL 94 HB-V1 |
Electrical
Property | Value |
---|---|
Dielectric constant | 3 [-] Show Material materials with Dielectric constant of 3 [-] |
3.2 [-] Show Material materials with Dielectric constant of 3.2 [-] | |
Electrical resistivity | 10000000000000 Ω·m Show Material materials with Electrical resistivity of 10000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Mouth guards, switch latches, fuseholders, breaker covers, dental x-ray holders | |
Processing methods | Injection molding, blow molding, extrusion, thermoforming |