General
Property | Value |
---|---|
Density | 0.83 - 0.84 g/cm³ Show Material materials with Density of 0.83 - 0.84 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 1.1 - 2.0 GPa Show Material materials with Elastic modulus of 1.1 - 2.0 GPa | |
Elongation | 12.0 - 60.0 % Show Material materials with Elongation of 12.0 - 60.0 % | |
Impact strength, Charpy unnotched | 15 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 15 kJ/m² | |
20 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m² | ||
Tensile strength | 10.0 - 30.0 MPa Show Material materials with Tensile strength of 10.0 - 30.0 MPa | at 5-7% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.000115 - 0.00038 1/K Show Material materials with Coefficient of thermal expansion of 0.000115 - 0.00038 1/K |
Melting point | 220.0 - 245.0 °C Show Material materials with Melting point of 220.0 - 245.0 °C |
Specific heat capacity | 2180 J/(kg·K) Show Material materials with Specific heat capacity of 2180 J/(kg·K) |
Thermal conductivity | 0.17 W/(m·K) Show Material materials with Thermal conductivity of 0.17 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2 [-] Show Material materials with Dielectric constant of 2 [-] |
2.12 [-] Show Material materials with Dielectric constant of 2.12 [-] | |
Electrical resistivity | 100000000000000.0 - 1000000000000000.0 Ω·m Show Material materials with Electrical resistivity of 100000000000000.0 - 1000000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | yes |
Technological properties
Property | ||
---|---|---|
Application areas | Sterilizable parts, packing for instant meals, automotive interior light fixtures, coloring spools, hollow fibres | |