Polypropylene Reinforced with 20% Talcum (PP+T40)

Alternative and trade names
Hostacom®, Altech®, Polyfort®
.XLSX
.PDF
Save

Description

High toughness

Properties

General

Density ρ

1.2 - 1.25 g/cm³ at 20 °C

Mechanical

Elastic modulus E

2.8 - 4.5 GPa at 20 °C

Elongation A

3 - 25 % at 20 °C

Impact strength, Charpy notched Ivnot

2 - 5 kJ/m² at 20 °C

Impact strength, Charpy unnotched Iunnot

15 - 55 kJ/m² at 20 °C

Max allowed stress σmax

26 - 35 MPa at 20 °C

at 2.5-4% strain

Thermal

Coefficient of thermal expansion α

6E-5 - 9E-5 1/K at 20 °C

Flammability

UL 94 HB

Melting point Tm

160 - 168 °C

Specific heat capacity cp

1390 J/(kg·K) at 20 °C

Thermal conductivity λ

0.56 W/(m·K) at 20 °C

Electrical

Dielectric constant εr

2.4 - 3 [-] at 20 °C

Electrical resistivity ρel

1.00E+13 - 1.00E+14 Ω·m at 20 °C

Optical

Transparency

no

Technological properties

Application areas

automotive instrument panels, washing machine parts

Fillers

40% Talcum

Processing methods

Injection molding, extrusion, thermoforming

This material data has been provided by M-Base.