Polycarbonate Reinforced with 20% Glass Fibre (PC+GF20)

Alternative and trade names
Makrolon®, Lupilon®, Edgetek™
.XLSX
.PDF
Save

Description

Reinforced Polycarbonate with 20% glass fiber with high viscosity and easy release.

Properties

General

Density ρ

1.3 - 1.35 g/cm³ at 20 °C

Mechanical

Elastic modulus E

5.6 - 6.5 GPa at 20 °C

Elongation A

2 - 4 % at 20 °C

Impact strength, Charpy notched Ivnot

6 - 13 kJ/m² at 20 °C

Impact strength, Charpy unnotched Iunnot

35 - 60 kJ/m² at 20 °C

Max allowed stress σmax

50 - 110 MPa at 20 °C

at 2-4% strain

Thermal

Coefficient of thermal expansion α

2.5E-5 - 7E-5 1/K at 20 °C

Flammability

UL 94 V2-V0

Max service temperature, long Tmaxlong

115 - 130 °C

Max service temperature, short Tmaxshort

115 - 150 °C

Thermal conductivity λ

0.23 - 0.34 W/(m·K) at 20 °C

Electrical

Dielectric constant εr

3.2 - 3.4 [-] at 20 °C

Electrical resistivity ρel

1.00E+13 - 1.00E+14 Ω·m at 20 °C

Optical

Transparency

no

Technological properties

Application areas

housing parts, handheld surgical devices, electrical components, electrical boxes

Fillers

20% Glass Fiber

Processing methods

Injection molding, extrusion

This material data has been provided by M-Base.