Polyamide 46 Reinforced with 30% Glass Fibre (PA46+GF30)

Alternative and trade names
Stanyl®
Want to keep this datasheet? Save it now in your required format

Description

Reinforced engineering polymer with 30% glass fiber. It is a high heat polyamide that offers excellent creep resistance, strength, stiffness and fatigue resistance not only at ambient temperatures but especially at high temperatures, while at the same time providing cycle-time advantages and excellent flow.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.41 - 1.43 g/cm³

Show Material materials with Density of 1.41 - 1.43 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

4.5 - 6.5 GPa

Show Material materials with Elastic modulus of 4.5 - 6.5 GPa

Elongation

4.0 - 8.0 %

Show Material materials with Elongation of 4.0 - 8.0 %

Impact strength, Charpy notched

15.0 - 21.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 15.0 - 21.0 kJ/m²

Impact strength, Charpy unnotched

60 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

100 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 100 kJ/m²

Tensile strength

110.0 - 120.0 MPa

Show Material materials with Tensile strength of 110.0 - 120.0 MPa

at 4-8% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2e-05 - 9e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 - 9e-05 1/K

Melting point

295 °C

Show Material materials with Melting point of 295 °C

Specific heat capacity

1700.0 - 1900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 1700.0 - 1900.0 J/(kg·K)

Thermal conductivity

0.24 - 0.33 W/(m·K)

Show Material materials with Thermal conductivity of 0.24 - 0.33 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

4.1 [-]

Show Material materials with Dielectric constant of 4.1 [-]

12 [-]

Show Material materials with Dielectric constant of 12 [-]

Electrical resistivity

1000000000.0 - 100000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000.0 - 100000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

air intake manifolds, aircraft engine components, echo muffler housing, oil suction pipes, power steering coils

Fillers

30% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding