General
Property | Value |
---|---|
Density | 1.18 - 1.2 g/cm³ Show Material materials with Density of 1.18 - 1.2 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 5.5 - 6.2 GPa Show Material materials with Elastic modulus of 5.5 - 6.2 GPa | |
Elongation | 2.0 - 3.0 % Show Material materials with Elongation of 2.0 - 3.0 % | |
Impact strength, Charpy notched | 5.0 - 8.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 5.0 - 8.0 kJ/m² | |
Impact strength, Charpy unnotched | 13 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 13 kJ/m² | |
21 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 21 kJ/m² | ||
Tensile strength | 65.0 - 80.0 MPa Show Material materials with Tensile strength of 65.0 - 80.0 MPa | at 2-3% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 3e-05 - 5e-05 1/K Show Material materials with Coefficient of thermal expansion of 3e-05 - 5e-05 1/K |
Thermal conductivity | 0.18 - 0.19 W/(m·K) Show Material materials with Thermal conductivity of 0.18 - 0.19 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.8 [-] Show Material materials with Dielectric constant of 2.8 [-] |
3.6 [-] Show Material materials with Dielectric constant of 3.6 [-] | |
Electrical resistivity | 1000000000000.0 - 100000000000000.0 Ω·m Show Material materials with Electrical resistivity of 1000000000000.0 - 100000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | electrical switches, furniture mounting brackets, electrical pump casings, automotive heater control valves | |
Fillers | 20% Glass Fiber | |
Processing methods | Injection molding, blow molding, extrusion |