General
Property | Value |
---|---|
Density | 1.68 - 1.7 g/cm³ Show Material materials with Density of 1.68 - 1.7 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 1.4 - 1.7 GPa Show Material materials with Elastic modulus of 1.4 - 1.7 GPa | |
Elongation | 150.0 - 450.0 % Show Material materials with Elongation of 150.0 - 450.0 % | |
Tensile strength | 28.0 - 31.0 MPa Show Material materials with Tensile strength of 28.0 - 31.0 MPa | at 5% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 7e-05 - 0.0001 1/K Show Material materials with Coefficient of thermal expansion of 7e-05 - 0.0001 1/K |
Melting point | 225.0 - 242.0 °C Show Material materials with Melting point of 225.0 - 242.0 °C |
Specific heat capacity | 1000 J/(kg·K) Show Material materials with Specific heat capacity of 1000 J/(kg·K) |
Thermal conductivity | 0.14 - 0.18 W/(m·K) Show Material materials with Thermal conductivity of 0.14 - 0.18 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.3 [-] Show Material materials with Dielectric constant of 2.3 [-] |
2.6 [-] Show Material materials with Dielectric constant of 2.6 [-] | |
Electrical resistivity | 10000000000000 Ω·m Show Material materials with Electrical resistivity of 10000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | yes |
Technological properties
Property | ||
---|---|---|
Application areas | cable sheathing, radio chemistry, chemical containers, fibers for fire-resistant upholstery | |
Processing methods | Injection molding, extrusion, coating |