General
Property | Value |
---|---|
Density | 1.49 - 1.51 g/cm³ Show Material materials with Density of 1.49 - 1.51 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 9.0 - 11.0 GPa Show Material materials with Elastic modulus of 9.0 - 11.0 GPa | |
Elongation | 2.0 - 3.0 % Show Material materials with Elongation of 2.0 - 3.0 % | |
Impact strength, Charpy notched | 10 kJ/m² Show Material materials with Impact strength, Charpy notched of 10 kJ/m² | |
Impact strength, Charpy unnotched | 40 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m² | |
Tensile strength | 150.0 - 165.0 MPa Show Material materials with Tensile strength of 150.0 - 165.0 MPa | at 2-3% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 2e-05 - 6e-05 1/K Show Material materials with Coefficient of thermal expansion of 2e-05 - 6e-05 1/K |
Thermal conductivity | 0.29 W/(m·K) Show Material materials with Thermal conductivity of 0.29 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 3.3 [-] Show Material materials with Dielectric constant of 3.3 [-] |
3.9 [-] Show Material materials with Dielectric constant of 3.9 [-] | |
Electrical resistivity | 100000000000000.0 - 1000000000000000.0 Ω·m Show Material materials with Electrical resistivity of 100000000000000.0 - 1000000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber | |
Processing methods | Injection molding |