Glass-fiber reinforced polyester engineering polymer molding compound. Very low mold shrinkage and post-shrinkage, very good mechanical strength, very good electrical values.

Properties

General

Density ρ

1.8 - 1.9 g/cm³ at 20 °C

Mechanical

Elastic modulus E

8 - 13 GPa at 20 °C

Elongation A

0.4 - 1.5 % at 20 °C

Impact strength, Charpy unnotched Iunnot

25 - 40 kJ/m² at 20 °C

Max allowed stress σmax

31 - 45 MPa at 20 °C

at 0.4-1.5% strain

Thermal

Coefficient of thermal expansion α

1.8E-5 1/K at 20 °C

Flammability

UL 94 HB

Max service temperature, long Tmaxlong

150 °C

Max service temperature, short Tmaxshort

210 °C

Specific heat capacity cp

1100 J/(kg·K) at 20 °C

Electrical

Dielectric constant εr

4.5 [-] at 20 °C

Electrical resistivity ρel

1.00E+1 Ω·m at 20 °C

Optical

Transparency

no

Technological properties

Application areas

lamp housings, iron housings, oven handles

Fillers

20% Glass Fiber

Processing methods

Compression molding, injection molding

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.