General
Property | Value |
---|---|
Density | 1.59 - 1.61 g/cm³ Show Material materials with Density of 1.59 - 1.61 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 12.0 - 14.5 GPa Show Material materials with Elastic modulus of 12.0 - 14.5 GPa | |
Elongation | 2.0 - 3.0 % Show Material materials with Elongation of 2.0 - 3.0 % | |
Impact strength, Charpy notched | 5 kJ/m² Show Material materials with Impact strength, Charpy notched of 5 kJ/m² | |
Impact strength, Charpy unnotched | 27 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 27 kJ/m² | |
Tensile strength | 205.0 - 220.0 MPa Show Material materials with Tensile strength of 205.0 - 220.0 MPa | at 2-3% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.000016 1/K Show Material materials with Coefficient of thermal expansion of 0.000016 1/K |
Specific heat capacity | 960 J/(kg·K) Show Material materials with Specific heat capacity of 960 J/(kg·K) |
Thermal conductivity | 0.36 W/(m·K) Show Material materials with Thermal conductivity of 0.36 W/(m·K) |
Flammability | UL 94 V0 |
Electrical
Property | Value |
---|---|
Dielectric constant | 4.4 [-] Show Material materials with Dielectric constant of 4.4 [-] |
Electrical resistivity | 2000000000000000 Ω·m Show Material materials with Electrical resistivity of 2000000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors, electrical housing, switches, valves | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection molding, extrusion |