Reinforced Styrene acrylonitrile with 50% glass fiber. It is a copolymer with high impact / impact modified.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.750 g/cm³

Show Material materials with Density of 1.750 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

24.5 - 35.7 GPa

Show Material materials with Elastic modulus of 24.5 - 35.7 GPa

Elongation

2.4 - 2.5 %

Show Material materials with Elongation of 2.4 - 2.5 %

Tensile strength

450.0 - 760.0 MPa

Show Material materials with Tensile strength of 450.0 - 760.0 MPa

at 2.4-2.5% strain

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Drones, orthoses, seat structures, interior trims

Fillers

48% Glass Fiber

Processing methods

Thermoforming, back injection molding