Polypropylene Reinforced with 70% Glass Fibers(PP+GF70), UD-Tape

Alternative and trade names
Udmax™
.XLSX
.PDF
Save

Description

Reinforced polypropylene PP with 70% glass fiber with high strength and stiffness, excellent processability & corrosion and fatigue resistance.

Properties

General

Density ρ

1.65 g/cm³ at 20 °C

Mechanical

Elastic modulus E

37 GPa at 20 °C

Elongation A

2.6 % at 20 °C

Max allowed stress σmax

948 MPa at 20 °C

at 2.6% strain

Thermal

Melting point Tm

163 °C

Optical

Transparency

no

Technological properties

Application areas

Truck bodies, vehicles, vehicle enclosures

Fillers

70% Glass Fiber

Processing methods

Thermoforming

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.