General
Property | Value |
---|---|
Density | 1.25 - 1.32 g/cm³ Show Material materials with Density of 1.25 - 1.32 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 8.2 - 11.0 GPa Show Material materials with Elastic modulus of 8.2 - 11.0 GPa | |
Elongation | 1.0 - 2.0 % Show Material materials with Elongation of 1.0 - 2.0 % | |
Impact strength, Charpy notched | 3.0 - 4.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 3.0 - 4.0 kJ/m² | |
Impact strength, Charpy unnotched | 11 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 11 kJ/m² | |
Tensile strength | 60.0 - 95.0 MPa Show Material materials with Tensile strength of 60.0 - 95.0 MPa | at 1-2% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.00005 1/K Show Material materials with Coefficient of thermal expansion of 0.00005 1/K |
Thermal conductivity | 0.17 W/(m·K) Show Material materials with Thermal conductivity of 0.17 W/(m·K) |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 2.5 [-] Show Material materials with Dielectric constant of 2.5 [-] |
Electrical resistivity | 100000000000000 Ω·m Show Material materials with Electrical resistivity of 100000000000000 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Housings | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection molding |