General
Property | Value |
---|---|
Density | 1.05 - 1.1 g/cm³ Show Material materials with Density of 1.05 - 1.1 g/cm³ |
Mechanical
Property | Value | Comment | |
---|---|---|---|
Elastic modulus | 0.9 - 1.7 GPa Show Material materials with Elastic modulus of 0.9 - 1.7 GPa | ||
Impact strength, Charpy notched | 10.0 - 75.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 10.0 - 75.0 kJ/m² | ||
Tensile strength | 35.0 - 60.0 MPa Show Material materials with Tensile strength of 35.0 - 60.0 MPa | at 15-20% strain | |
Impact strength, Charpy unnotched | no break |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 7e-05 - 0.00014 1/K Show Material materials with Coefficient of thermal expansion of 7e-05 - 0.00014 1/K |
Melting point | 250 °C Show Material materials with Melting point of 250 °C |
Electrical
Property | Value |
---|---|
Electrical resistivity | 700000000000.0 - 1000000000000.0 Ω·m Show Material materials with Electrical resistivity of 700000000000.0 - 1000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Engine covers, window insulating profiles, crankshaft covers | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, extrusion |