General
Property | Value |
---|---|
Density | 1.05 - 1.15 g/cm³ Show Material materials with Density of 1.05 - 1.15 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 3.2 - 5.1 GPa Show Material materials with Elastic modulus of 3.2 - 5.1 GPa | |
Elongation | 1.5 - 2.5 % Show Material materials with Elongation of 1.5 - 2.5 % | |
Impact strength, Charpy notched | 4.0 - 5.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 4.0 - 5.0 kJ/m² | |
Impact strength, Charpy unnotched | 10 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 10 kJ/m² | |
25 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 25 kJ/m² | ||
Tensile strength | 20.0 - 45.0 MPa Show Material materials with Tensile strength of 20.0 - 45.0 MPa | at 1.5-2.5% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 0.00005 1/K Show Material materials with Coefficient of thermal expansion of 0.00005 1/K |
Thermal conductivity | 0.25 - 0.26 W/(m·K) Show Material materials with Thermal conductivity of 0.25 - 0.26 W/(m·K) |
Flammability | UL 94 HB |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Furniture legs, buttons, reels | |
Fillers | 50% Wood Powder | |
Other | You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application: Polymer Advanced Search | |
Processing methods | Injection molding, extrusion |