General
Property | Value |
---|---|
Density | 1.2 - 1.4 g/cm³ Show Material materials with Density of 1.2 - 1.4 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 0.85 - 3.0 GPa Show Material materials with Elastic modulus of 0.85 - 3.0 GPa | |
Elongation | 2.0 - 15.0 % Show Material materials with Elongation of 2.0 - 15.0 % | |
Impact strength, Charpy unnotched | 5 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 5 kJ/m² | |
100 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | ||
Tensile strength | 15.0 - 35.0 MPa Show Material materials with Tensile strength of 15.0 - 35.0 MPa | at 2-15% strain |
Thermal
Property | Value |
---|---|
Melting point | 145.0 - 155.0 °C Show Material materials with Melting point of 145.0 - 155.0 °C |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Biodegradable packaging, biodegradable horticulture | |
Processing methods | Injection molding, extrusion, thermoforming, calandering |