Description

It is a high impact amorphous thermoplastic blends combine ease of processing with low-temperature ductility. With excellent impact resistance, heat resistance, and outstanding aesthetics. It provides an excellent design solution when both appearance and durability are important.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.06 - 1.17 g/cm³

Show Material materials with Density of 1.06 - 1.17 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

2.0 - 2.6 GPa

Show Material materials with Elastic modulus of 2.0 - 2.6 GPa

Elongation

50.0 - 100.0 %

Show Material materials with Elongation of 50.0 - 100.0 %

Impact strength, Charpy notched

30.0 - 65.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 30.0 - 65.0 kJ/m²

Impact strength, Charpy unnotched

40 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 40 kJ/m²

Tensile strength

40.0 - 60.0 MPa

Show Material materials with Tensile strength of 40.0 - 60.0 MPa

at 3-5% strain

Thermal

PropertyValue

Coefficient of thermal expansion

5e-05 - 0.0001 1/K

Show Material materials with Coefficient of thermal expansion of 5e-05 - 0.0001 1/K

Melting point

260 °C

Show Material materials with Melting point of 260 °C

Thermal conductivity

0.2 W/(m·K)

Show Material materials with Thermal conductivity of 0.2 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

3 [-]

Show Material materials with Dielectric constant of 3 [-]

3.1 [-]

Show Material materials with Dielectric constant of 3.1 [-]

Electrical resistivity

10000000000000.0 - 100000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 10000000000000.0 - 100000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Electroplating applications, mobilephone housings, power supply boxes

Processing methods