Polycarbonate Reinforced with 10% Glass Fibers (PC+GF10)

Alternative and trade names
Makrolon®, Lexan®
.XLSX
.PDF
Save

Description

Reinforced polycarbonate with 10% glass fiber. low and high viscosity, easy release, flame retardant and UV stabilized grades are available.

Properties

General

Density ρ

1.24 - 1.27 g/cm³ at 20 °C

Mechanical

Elastic modulus E

2.7 - 4.5 GPa at 20 °C

Elongation A

2 - 15 % at 20 °C

Impact strength, Charpy notched Ivnot

6 - 14 kJ/m² at 20 °C

Impact strength, Charpy unnotched Iunnot

45 kJ/m² at 20 °C

no break

Max allowed stress σmax

45 - 85 MPa at 20 °C

at 2-15% strain

Thermal

Coefficient of thermal expansion α

3E-5 - 7E-5 1/K at 20 °C

Flammability

UL 94 V2-V0

Max service temperature, long Tmaxlong

115 - 130 °C

Max service temperature, short Tmaxshort

115 - 150 °C

Thermal conductivity λ

0.21 - 0.22 W/(m·K) at 20 °C

Electrical

Dielectric constant εr

2.8 - 3.2 [-] at 20 °C

Electrical resistivity ρel

1.00E+13 - 1.00E+14 Ω·m at 20 °C

Optical

Transparency

no

Technological properties

Application areas

Housing parts

Fillers

10% Glass Fiber

Processing methods

Injection molding, extrusion

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.