Poly-M-Xylylenadipamid Reinforced with 30% Glass Fibers (PAMXD6+GF30)

Alternative and trade names
Reny®, Terez
Want to keep this datasheet? Save it now in your required format

Description

It is a reinforced Poly-M-Xylylenadipamid with 30% glass fiber. The key features are:


  • Excellent mechanical strength and elastic modulus over a wide range of temperatures
  • Lower water absorption compared to commodity polyamides showing decrease in dimensional and mechanical strength change under water absorption condition
  • High heat distortion temperature, low thermal expansion coefficient, equivalent to metal alloys
  • Excellent chemical resistance against oils and organic solvents
  • Low mold shrinkage and low warpage, suitable for precise mold articles
  • Good surface finish even in high glass fiber content
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.42 - 1.46 g/cm³

    Show Material materials with Density of 1.42 - 1.46 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    11.1 - 11.8 GPa

    Show Material materials with Elastic modulus of 11.1 - 11.8 GPa

    Elongation

    2.0 - 2.5 %

    Show Material materials with Elongation of 2.0 - 2.5 %

    Impact strength, Charpy notched

    6.0 - 7.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 6.0 - 7.0 kJ/m²

    Impact strength, Charpy unnotched

    30 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 30 kJ/m²

    50 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 50 kJ/m²

    Tensile strength

    140.0 - 185.0 MPa

    Show Material materials with Tensile strength of 140.0 - 185.0 MPa

    at 2-2.5% strain

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    1.5e-05 - 5e-05 1/K

    Show Material materials with Coefficient of thermal expansion of 1.5e-05 - 5e-05 1/K

    Melting point

    235.0 - 240.0 °C

    Show Material materials with Melting point of 235.0 - 240.0 °C

    Flammability

    UL 94 HB

    Electrical

    PropertyValue

    Dielectric constant

    4 [-]

    Show Material materials with Dielectric constant of 4 [-]

    5 [-]

    Show Material materials with Dielectric constant of 5 [-]

    Electrical resistivity

    10000000000000.0 - 20000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 10000000000000.0 - 20000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Fillers

    30% Glass Fiber

    Processing methods

    Injection molding