General
Property | Value |
---|---|
Density | 1.7 - 1.72 g/cm³ Show Material materials with Density of 1.7 - 1.72 g/cm³ |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 12.0 - 13.0 GPa Show Material materials with Elastic modulus of 12.0 - 13.0 GPa | |
Elongation | 1.5 - 3.0 % Show Material materials with Elongation of 1.5 - 3.0 % | |
Impact strength, Charpy notched | 5.0 - 10.0 kJ/m² Show Material materials with Impact strength, Charpy notched of 5.0 - 10.0 kJ/m² | |
Impact strength, Charpy unnotched | 20 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 20 kJ/m² | |
25 kJ/m² Show Material materials with Impact strength, Charpy unnotched of 25 kJ/m² | ||
Tensile strength | 120.0 - 140.0 MPa Show Material materials with Tensile strength of 120.0 - 140.0 MPa | at 1.5-3% strain |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 2e-05 - 7e-05 1/K Show Material materials with Coefficient of thermal expansion of 2e-05 - 7e-05 1/K |
Melting point | 165.0 - 167.0 °C Show Material materials with Melting point of 165.0 - 167.0 °C |
Flammability | UL 94 HB |
Electrical
Property | Value |
---|---|
Dielectric constant | 4.2 [-] Show Material materials with Dielectric constant of 4.2 [-] |
4.5 [-] Show Material materials with Dielectric constant of 4.5 [-] | |
Electrical resistivity | 1000000000000.0 - 100000000000000.0 Ω·m Show Material materials with Electrical resistivity of 1000000000000.0 - 100000000000000.0 Ω·m |
Optical
Property | Value |
---|---|
Transparency | no |
Technological properties
Property | ||
---|---|---|
Application areas | Casings of pumps, pivot bearings | |
Fillers | 40% Glass Fiber | |
Processing methods | Injection molding |