Description

Oerlikon Metco’s nickel-chromium based superalloy powders produce dense, self-bonding, single-step coatings that are oxidation and corrosion resistant at elevated temperatures.


Their compositions are similar to Inconels, thus the coatings have excellent high temperature oxidation and corrosion resistance for restoration and repair of superalloy components. They are also recommended as overlay coatings to protect less noble materials from oxidation.


The coatings exhibit high tensile bond strength and thickness limits exceeding 1.5 - 2.5 mm (0.06 - 0.1 in) when sprayed with liquid-fuel or gas-fuel HVOF guns, depending on part geometry. The coatings can be machined, milled, drilled and tapped without chipping and excellent edge retention.


The materials Amdry™ 718, Amdry 718 Cl.B, Amdry 1718 and Diamalloy™ 1006 of this material family differ primarily in their particle size distribution and are all manufactured via gas atomization.


Discover Amdry™ 718 online at myMetco. View current product pricing and availability.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size range

11 - 125 µm

Show Supplier Material materials with Particle size range of 11 - 125 µm

Amdry™ 718 -125 +45µm, Amdry 718 Cl.B -90 +45µm, Amdry 1718 -45 +15µm, Diamalloy™ 1006 -45 +11µm

Thermal

PropertyValue

Max service temperature

704 °C

Show Supplier Material materials with Max service temperature of 704 °C

Chemical properties

PropertyValue

Aluminium

0.5 %

Show Supplier Material materials with Aluminium of 0.5 %

Carbon

0.05 %

Show Supplier Material materials with Carbon of 0.05 %

Chromium

19 %

Show Supplier Material materials with Chromium of 19 %

Iron

18 %

Show Supplier Material materials with Iron of 18 %

Molybdenum

3 %

Show Supplier Material materials with Molybdenum of 3 %

Nickel

balance

Niobium + Tantalum

5.1 %

Show Supplier Material materials with Niobium + Tantalum of 5.1 %

Titanium

0.95 %

Show Supplier Material materials with Titanium of 0.95 %

Technological properties

Property
Application areas

Repair and restoration of mis-machined and worn superalloy components, Gas turbine components, Chemical processing equipment, Pollution control equipment, Pump bodies, Extrusion dies, Rocket engine components

Availability

Stock

Chemical composition

Ni 19Cr 18Fe 3Mo 5(Nb+Ta) 0.5Al

Distribution

Global

Handling recommendations

Store in the original container in a dry location; Tumble contents gently prior to use to prevent segregation; Open containers should be stored in a drying oven to prevent moisture pickup; Remove desiccant prior to use, if applicable.

Morphology

Spheroidal

Order number

Amdry™ 718: 1001047, Amdry 718 Cl.B: 1001048, Amdry 1718, Diamalloy™ 1006: 1001063

Other

Designed for restoration of worn or mismatched components of Inconel 713C, Inconel 718 or similar substrates. These materials have identical chemical compositions and are similar to Inconel 718 which has a typical bulk service temperature up to 704 °C (1300 °F). The materials differ primarily in their particle size distribution which has been optimized for various spray guns

Packaging size

5 lb (approx. 2.25 kg)

Processing history

Gas atomized

Processing methods

Atmospheric Plasma Spray, HVOF