Description

Oerlikon Metco’s CoCr[NiWSi]C products are inert gas atomized powders that are chemically homogeneous, exhibit minimal satellites and are freely flowing. They are designed and provide excellent results for a variety of applications such as laser cladding, thermal spray and PTA. These materials form coatings that are appropriate for wear and corrosion resistance in relatively high-temperature service conditions.


Metco 1220 series materials have chemical compositions similar to that of Stellite 6. Metco 1220 series materials are designed for laser cladding.


Discover Metco 1220C online at myMetco. View current product pricing and availability.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size range

20 - 53 µm

Show Supplier Material materials with Particle size range of 20 - 53 µm

Nominal range -53 +20µm: +5% 53µm, -5% 20µm

Thermal

PropertyValue

Melting point

1260 - 1357 °C

Show Supplier Material materials with Melting point of 1260 - 1357 °C

Chemical properties

PropertyValueComment

Carbon

1.08 %

Show Supplier Material materials with Carbon of 1.08 %

Chromium

28.5 %

Show Supplier Material materials with Chromium of 28.5 %

Cobalt

balance

Iron

3 %

Show Supplier Material materials with Iron of 3 %

max

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

max

Silicon

1.6 %

Show Supplier Material materials with Silicon of 1.6 %

Tungsten

4.5 %

Show Supplier Material materials with Tungsten of 4.5 %

Technological properties

Property
Availability

Stock

Chemical composition

CoCrWFeSiC

Distribution

Global

Morphology

Spheroidal

Order number

1301058

Other

Deposits have good resistance to seizing, galling and cavitation over a wide temperature range, and combat adhesive, abrasive or erosive wear combined with corrosion at relatively high temperatures. They provide good thermal oxidation resistance at temperatures up to 1000°C (1800 °F). Deposits resist oxidizing acids, but perform poorly in strong reducing acids such as hydrochloric with the degree of resistance dependant on the acidic concentration and temperature. Self-mating surfaces exhibit a very low coefficient of friction (≈ 0.12). Choose Metco 1220C for deposits as thin as 0.5 mm (0.02 in). Its finer particle size distribution can save processing time and cost, as the time to grind to dimension is reduced.

Packaging size

5 kg (approx. 11 lb)

Processing history

Gas atomized

Processing methods

Atmospheric Plasma Spray, Laser Cladding

Safety data sheet