Description

Oerlikon Metco’s CoCr[NiWSi]C products are inert gas atomized powders that are chemically homogeneous, exhibit minimal satellites and are freely flowing. They are designed and provide excellent results for a variety of applications such as laser cladding, thermal spray and PTA. These materials form coatings that are appropriate for wear and corrosion resistance in relatively high-temperature service conditions.


Diamalloy 4060NS has a chemical composition similar to that of Stellite 6. Diamalloy 4060NS is designed for HVOF applications.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size range

11 - 45 µm

Show Supplier Material materials with Particle size range of 11 - 45 µm

Nominal range -45 +11µm: +5% 45µm, -2% 11µm

Thermal

PropertyValue

Melting point

1260 - 1357 °C

Show Supplier Material materials with Melting point of 1260 - 1357 °C

Chemical properties

PropertyValueComment

Carbon

1.08 %

Show Supplier Material materials with Carbon of 1.08 %

Chromium

28.5 %

Show Supplier Material materials with Chromium of 28.5 %

Cobalt

balance

Iron

3 %

Show Supplier Material materials with Iron of 3 %

max

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

max

Silicon

1.6 %

Show Supplier Material materials with Silicon of 1.6 %

Tungsten

4.5 %

Show Supplier Material materials with Tungsten of 4.5 %

Technological properties

Property
Availability

Stock

Chemical composition

CoCrWFeSiC

Distribution

Global

Morphology

Spheroidal

Order number

10 lb (approx. 4.5 kg): 1037003; 5 kg (approx. 11 lb): 1300203

Other

Diamalloy 4060NS is used as a general restoration and repair material when compatibility with Stellite 6 is desired. When applied using HVOF, it forms dense, wear-resistant and oxidation-resistant coatings that may be used for turbine hot section applications such as combustion liners

Packaging size

10 lb (approx. 4.5 kg), 5 kg (approx. 11 lb)

Processing history

Gas atomized

Processing methods

High Velocity Oxygen Fuel Spray (HVOF), Atmospheric Plasma Spray, Combustion Powder Thermospray