Amdry 625 Nickel Chromium Superalloy Atomized Thermal Spray Powder

Alternative and trade names
similar to Inconel 625 (Inconel is a registered trademark of Huntington Alloys Corp.), Diamalloy 1005, Diamalloy 1005A
Want to keep this datasheet? Save it now in your required format

Description

Oerlikon Metco’s nickel-chromium based superalloy powders produce dense, self-bonding, single-step coatings that are oxidation and corrosion resistant at elevated temperatures.


Their compositions are similar to Inconels, thus the coatings have excellent high temperature oxidation and corrosion resistance for restoration and repair of superalloy components. They are also recommended as overlay coatings to protect less noble materials from oxidation.


The coatings exhibit high tensile bond strength and thickness limits exceeding 1.5 - 2.5 mm (0.06 - 0.1 in) when sprayed with liquid-fuel or gas-fuel HVOF guns, depending on part geometry. The coatings can be machined, milled, drilled and tapped without chipping and excellent edge retention.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Particle size range

45 - 90 µm

Show Supplier Material materials with Particle size range of 45 - 90 µm

Thermal

PropertyValue

Max service temperature

982 °C

Show Supplier Material materials with Max service temperature of 982 °C

Chemical properties

PropertyValue

Chromium

21.5 %

Show Supplier Material materials with Chromium of 21.5 %

Iron

2.5 %

Show Supplier Material materials with Iron of 2.5 %

Molybdenum

9 %

Show Supplier Material materials with Molybdenum of 9 %

Nickel

balance

Niobium + Tantalum

3.7 %

Show Supplier Material materials with Niobium + Tantalum of 3.7 %

Technological properties

Property
Application areas

Repair and restoration of mis-machined and worn superalloy components, Gas turbine components, Chemical processing equipment, Pollution control equipment, Pump bodies, Extrusion dies, Rocket engine components

Availability

Stock

Chemical composition

Ni 21.5Cr 2.5Fe 9Mo 3.7(Nb+Ta)

Distribution

Global

Handling recommendations

Store in the original container in a dry location; Tumble contents gently prior to use to prevent segregation; Open containers should be stored in a drying oven to prevent moisture pickup; Remove desiccant prior to use, if applicable.

Morphology

Spheroidal

Order number

1001045

Other

Designed for restoration of worn or mismatched components of Inconel 625 or similar substrates. Amdry 625 is sized for plasma spray.

Packaging size

5 lb (approx. 2.25 kg)

Processing history

Gas atomized

Processing methods

Atmospheric Plasma Spray

Safety data sheet

www.oerlikon.com/metco SDS No. 50-310