Amdry MM509-C Cobalt Chromium Nickel Tungsten Alloy Powder

Alternative and trade names
similar to Mar M 509, Amdry MM509
Want to keep this datasheet? Save it now in your required format

Description

Oerlikon Metco’s CoCr[NiWSi]C products are inert gas atomized powders that are chemically homogeneous, exhibit minimal satellites and are freely flowing. They are designed and provide excellent results for a variety of applications such as laser cladding, thermal spray and PTA. These materials form coatings that are appropriate for wear and corrosion resistance in relatively high-temperature service conditions.


Amdry MM509 series is similar in chemistry to Mar M 509 cast alloy and is best applied using atmospheric plasma spray.


Amdry MM509 series can also be used as complimentary additive to Oerlikon Metco's ADB brazing alloys to facilitate crack and surface repairs.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Particle size range

45 - 125 µm

Show Supplier Material materials with Particle size range of 45 - 125 µm

Nominal range -125 +45µm: +5% 125µm, -15% 45µm

Thermal

PropertyValue

Melting point

1383 - 1454 °C

Show Supplier Material materials with Melting point of 1383 - 1454 °C

Chemical properties

PropertyValueComment

Carbon

0.6 %

Show Supplier Material materials with Carbon of 0.6 %

Chromium

23.5 %

Show Supplier Material materials with Chromium of 23.5 %

Cobalt

balance

Nickel

10 %

Show Supplier Material materials with Nickel of 10 %

Other

0.3 %

Show Supplier Material materials with Other of 0.3 %

max

Tantalum

3.5 %

Show Supplier Material materials with Tantalum of 3.5 %

Titanium

0.23 %

Show Supplier Material materials with Titanium of 0.23 %

Tungsten

7 %

Show Supplier Material materials with Tungsten of 7 %

Zirconium

0.45 %

Show Supplier Material materials with Zirconium of 0.45 %

Technological properties

Property
Availability

Stock

Chemical composition

CoCrNiWTaCZrTi

Distribution

Global

Handling recommendations

Store in the original container in a dry location; Tumble contents prior to use to prevent segregation. Open containers should be stored in a drying oven to prevent moisture pickup.

Morphology

Spheroidal

Order number

1059330

Other

These products were designed as complimentary filler metals for repair and wide-gap brazing applications. Amdry MM509-C is similar to Mar M 509 casting alloy that contains carbide-forming elements. As coatings, it is best applied using atmospheric plasma spray and is primarily used for surface restoration of worn or damaged gas turbine parts such as airfoils, combustors, blades and vanes.

Packaging size

10 lb (approx. 4.5 kg)

Processing history

Gas atomized

Processing methods

Atmospheric Plasma Spray, Laser Cladding, PTA, Brazing

Safety data sheet

www.oerlikon.com/metco SDS No. 50-1023