Diamalloy 1013 Austenitic Stainless Steel Powder for Thermal Spray

Alternative and trade names
similar to Type 316L
Want to keep this datasheet? Save it now in your required format

Description

Diamalloy 1013 is an austenitic, nickel-chromium stainless steel powder, similar to Type 316L. It produces thermal sprayed coatings that are bright, dense and resistant to corrosion and wear. These coatings can easily be machined to a very good finish with ordinary steel tools.


The dense coatings produced by this product is particularly recommended for applications that require protection against corrosion, cavitation and mild particle erosion at ­temperatures less than 540 °C (1000 °F). These coatings are also used for the salvage and build up of worn or mismachined steel parts. In addition, these coatings work-harden in service, making them suitable for packing areas on pump shafts and bearing surfaces on motor shafts.


Coatings of these materials contain enough molybdenum to guarantee particularly high resistance to pitting and crevice corrosion in chloride environments, and they also exhibit high impact resistance and tensile strength at elevated temperatures.

Related Standards

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Particle size range

20 - 53 µm

Show Supplier Material materials with Particle size range of 20 - 53 µm

Thermal

PropertyValue

Max service temperature

540 °C

Show Supplier Material materials with Max service temperature of 540 °C

Chemical properties

PropertyValueComment

Carbon

0.03 %

Show Supplier Material materials with Carbon of 0.03 %

max

Chromium

17 %

Show Supplier Material materials with Chromium of 17 %

Iron

balance

Molybdenum

2.5 %

Show Supplier Material materials with Molybdenum of 2.5 %

Nickel

12 %

Show Supplier Material materials with Nickel of 12 %

Silicon

0.75 %

Show Supplier Material materials with Silicon of 0.75 %

Technological properties

Property
Application areas

Corrosion: Rolls used in the printing industry, Pump plungers, Shafts, Seal rings, Impellers, Hydraulic rams, Cavitation: Wear rings on hydraulic turbines, Diesel engine cylinder liners, Pumps, Low temperature particle erosion: Exhaust fans, Hydraulic valves, Cyclone dust collectors, Dump valve plugs and seats, Salvage/buildup on mismachined or worn steel parts

Availability

Special Order

Chemical composition

Fe 12Ni 17Cr 2.5Mo 0.75Si 0.03C

Distribution

Global

Handling recommendations

Store in the original container in a dry location; Tumble contents gently prior to use to prevent segregation; Open containers should be stored in a drying oven to prevent moisture pickup.

Morphology

Spheroidal

Order number

1092413

Other

Diamalloy 1013 is designed for application using HVOF. It produces coatings that are smoother, denser and less oxidized than coatings of ­Metco 41-series, and are more suitable for corrosion applications. The low carbon and silicon content of Diamalloy 1013 produces coatings with better corrosion protection in weld-type applications (less prone to sensitization).

Packaging size

5 kg (approx. 11 lb)

Processing history

Gas atomized

Processing methods

HVOF