Amdry MM509B-F Cobalt Braze Alloy Powder (Boron as Melt-Depressant)

Alternative and trade names
similar to MarM-509, Amdry MM509B-C
Want to keep this datasheet? Save it now in your required format

Description

The Amdry™ MM509 series of alloy powders are spherical, inert gas atomized, cobalt-based powders.


Amdry MM509B-F is chemically similar to MarM-509, but contains boron as a melt-depressant. It is commonly used as activated diffusion braze alloy for the repair of cobalt-based components.


The Amdry™ MM509 series can also be used in thermal spray coating applications. Gas atomization ensures excellent chemical homogeneity and high purity for consistent processing results.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Particle size range

5 - 45 µm

Show Supplier Material materials with Particle size range of 5 - 45 µm

Chemical properties

PropertyValue

Boron

2 - 3 %

Show Supplier Material materials with Boron of 2 - 3 %

Carbon

0.55 - 0.65 %

Show Supplier Material materials with Carbon of 0.55 - 0.65 %

Chromium

22.5 - 24.25 %

Show Supplier Material materials with Chromium of 22.5 - 24.25 %

Cobalt

balance

Nickel

9 - 11 %

Show Supplier Material materials with Nickel of 9 - 11 %

Tantalum

3 - 4 %

Show Supplier Material materials with Tantalum of 3 - 4 %

Titanium

0.15 - 0.3 %

Show Supplier Material materials with Titanium of 0.15 - 0.3 %

Tungsten

6.5 - 7.5 %

Show Supplier Material materials with Tungsten of 6.5 - 7.5 %

Zirconium

0.3 - 0.6 %

Show Supplier Material materials with Zirconium of 0.3 - 0.6 %

Technological properties

Property
Application areas

Blend material for braze repairs, such as restoration of worn or damaged areas, crack repair or repair of surface defects. Joining of cobalt-based superalloy components for use in high temperature service conditions. Applications where excellent joint strength is required. Wide-gap braze applications by blending Amdry MM509 with Amdry MM509B-C or Amdry MM509B-F. Thermal spray coating for superalloy components. Used on aerospace and industrial gas turbine components.

Availability

Stock

Chemical composition

Co 24Cr 10Ni 7W 3.5Ta 0.6C 2.5B

Distribution

Global

Handling recommendations

Store in the original, closed container in a dry location; Tumble contents prior to use to prevent segregation.

Morphology

Spheroidal

Order number

1030109

Other

Amdry MM509B-F can be used as activated diffusion braze alloys. It can be blended with Amdry MM509, Amdry MM509-C or other Amdry superalloy matrix materials. Please refer to customer specification requirements or contact Oerlikon Metco for specific blend ratios.

Packaging size

10 lb (approx. 4.5 kg)

Processing history

Gas atomized

Processing methods

Diffusion Brazing