General
Property | Value |
---|---|
Particle size range | 45 - 90 µm Show Supplier Material materials with Particle size range of 45 - 90 µm |
Chemical properties
Property | ||
---|---|---|
Chromium | 20 - 23 % | |
Iron | 5 % | max |
Molybdenum | 8 - 10 % | |
Nickel | balance | |
Niobium + Tantalum | 3.15 - 4.15 % | |
Other | 3.53 % | max |
Technological properties
Property | ||
---|---|---|
Application areas | Blended in various ratios with ADB braze filler metals for crack repair and surface restoration on superalloy turbine airfoils and other turbine components. General repair and restoration of superalloy-based components. Blended in various ratios with standard braze filler to form excellent wide-gap filler metals. | |
Availability | Stock | |
Chemical composition | Ni 21.5Cr 9Mo 3.6(Nb+Ta) 2.5Fe | |
Distribution | Global | |
Handling recommendations | Store in the original, closed container in a dry location and Tumble contents prior to use to prevent segregation. | |
Morphology | Spheroidal | |
Order number | 1001045 | |
Packaging size | 5 lb (approx. 2.25 kg) | |
Processing history | Gas Atomized | |
Processing methods | Brazing | |
Safety data sheet | www.oerlikon.com/metco SDS No. 50-310 |