Amdry™ nickel and cobalt superalloy powders were developed as complimentary additives for Metco ADB (Activated Diffusion Braze) filler metals, such as Amdry DF-3, DF-4B, DF-6A or BRB, for crack repair and surface restoration. These superalloy products are produced by a dry gas atomization process to assure consistency, purity and conformity to rigid industrial, aerospace and military specifications.


Regardless of the base material that required brazing or repair, the wide range of Metco superalloy powders ensures the right choice and availability.


Metco superalloy products are produced and available as powders. While blending is typically performed by the customer, any ratios desired can be pre-blended for you by Oerlikon Metco. The powders can be delivered pre-blended with braze alloy powders for use with cements or gels. The blends can also be converted to paste, braze tape or braze preforms for a more precise and cost-effective method of application.


Amdry superalloy products do not contain temperature suppressants. Therefore, they are designed not to melt during the braze process, but to form a matrix within the braze joint that is metallurgically compatible with the substrate material.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Particle size range

45 - 125 µm

Show Supplier Material materials with Particle size range of 45 - 125 µm

Chemical properties

PropertyValueComment

Aluminium

0.3 - 0.7 %

Show Supplier Material materials with Aluminium of 0.3 - 0.7 %

Carbon

0.02 - 0.08 %

Show Supplier Material materials with Carbon of 0.02 - 0.08 %

Chromium

17 - 21 %

Show Supplier Material materials with Chromium of 17 - 21 %

Iron

15 - 21 %

Show Supplier Material materials with Iron of 15 - 21 %

Molybdenum

2.8 - 3 %

Show Supplier Material materials with Molybdenum of 2.8 - 3 %

Nickel

50 - 55 %

Show Supplier Material materials with Nickel of 50 - 55 %

Niobium + Tantalum

4.75 - 5.5 %

Show Supplier Material materials with Niobium + Tantalum of 4.75 - 5.5 %

Other

2.12 %

Show Supplier Material materials with Other of 2.12 %

max

Titanium

0.75 - 1.15 %

Show Supplier Material materials with Titanium of 0.75 - 1.15 %

Technological properties

Property
Application areas

Blended in various ratios with ADB braze filler metals for crack repair and surface restoration on superalloy turbine airfoils and other turbine components. General repair and restoration of superalloy-based components. Blended in various ratios with standard braze filler to form excellent wide-gap filler metals.

Availability

Stock

Chemical composition

Ni 19Cr 18Fe 3Mo 5(Nb+Ta) 0.5Al 1Ti 0.05C

Distribution

Global

Handling recommendations

Store in the original, closed container in a dry location and Tumble contents prior to use to prevent segregation.

Morphology

Spheroidal

Order number

1001047

Packaging size

5 lb (approx. 2.25 kg)

Processing history

Gas Atomized

Processing methods

Brazing