Amdry Rene 80 Superalloy Powder for Braze Repair

Alternative and trade names
similar to Rene 80 (Rene is a registered trademark of Teledyne Industries, Inc.)
Want to keep this datasheet? Save it now in your required format

Description

Amdry™ nickel and cobalt superalloy powders were developed as complimentary additives for Metco ADB (Activated Diffusion Braze) filler metals, such as Amdry DF-3, DF-4B, DF-6A or BRB, for crack repair and surface restoration. These superalloy products are produced by a dry gas atomization process to assure consistency, purity and conformity to rigid industrial, aerospace and military specifications.


Regardless of the base material that required brazing or repair, the wide range of Metco superalloy powders ensures the right choice and availability.


Metco superalloy products are produced and available as powders. While blending is typically performed by the customer, any ratios desired can be pre-blended for you by Oerlikon Metco. The powders can be delivered pre-blended with braze alloy powders for use with cements or gels. The blends can also be converted to paste, braze tape or braze preforms for a more precise and cost-effective method of application.


Amdry superalloy products do not contain temperature suppressants. Therefore, they are designed not to melt during the braze process, but to form a matrix within the braze joint that is metallurgically compatible with the substrate material.

This material data has been provided by Oerlikon Metco.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Particle size range

45 - 125 µm

Show Supplier Material materials with Particle size range of 45 - 125 µm

Chemical properties

PropertyValueComment

Aluminium

2.8 - 3.2 %

Show Supplier Material materials with Aluminium of 2.8 - 3.2 %

Boron

0.01 - 0.02 %

Show Supplier Material materials with Boron of 0.01 - 0.02 %

Carbon

0.15 - 0.19 %

Show Supplier Material materials with Carbon of 0.15 - 0.19 %

Chromium

13.7 - 14.3 %

Show Supplier Material materials with Chromium of 13.7 - 14.3 %

Cobalt

9 - 10 %

Show Supplier Material materials with Cobalt of 9 - 10 %

Molybdenum

3.7 - 4.3 %

Show Supplier Material materials with Molybdenum of 3.7 - 4.3 %

Nickel

balance

Other

3.43 %

Show Supplier Material materials with Other of 3.43 %

max

Titanium

4.8 - 5.2 %

Show Supplier Material materials with Titanium of 4.8 - 5.2 %

Tungsten

3.7 - 4.3 %

Show Supplier Material materials with Tungsten of 3.7 - 4.3 %

Technological properties

Property
Application areas

Blended in various ratios with ADB braze filler metals for crack repair and surface restoration on superalloy turbine airfoils and other turbine components. General repair and restoration of superalloy-based components. Blended in various ratios with standard braze filler to form excellent wide-gap filler metals.

Availability

Stock

Chemical composition

Ni 14Cr 9.5Co 5Ti 4Mo 4W 3Al 0.17C

Distribution

Global

Handling recommendations

Store in the original, closed container in a dry location and Tumble contents prior to use to prevent segregation.

Morphology

Spheroidal

Order number

1005578

Packaging size

5 lb (approx. 2.25 kg)

Processing history

Gas Atomized

Processing methods

Brazing

Safety data sheet

www.oerlikon.com/metco SDS No. 50-775